SAE AMS4217G-1996
Aluminum Alloy, Castings 7Si 0.3Mg, Solution and Precipitation Heat Treated

Standard No.
SAE AMS4217G-1996
Release Date
1996
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4217H-2007
Latest
SAE AMS4217J-2018
Scope
This specification covers an aluminum alloy in the form of castings. These castings have been used typically for components requiring high strength at room temperature, but usage is not limited to such applications.

SAE AMS4217G-1996 history

  • 2018 SAE AMS4217J-2018 Aluminum Alloy@ Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
  • 2012 SAE AMS4217H-2012 Aluminum Alloy, Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated
  • 2007 SAE AMS4217H-2007 Aluminum Alloy, Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated UNS A03560
  • 1996 SAE AMS4217G-1996 Aluminum Alloy, Castings 7Si 0.3Mg, Solution and Precipitation Heat Treated
  • 1995 SAE AMS4217F-1995 ALUMINUM ALLOY CASTINGS, SAND 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated
  • 1986 SAE AMS4217F-1986 ALUMINUM ALLOY CASTINGS@ SAND 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
  • 1978 SAE AMS4217E-1978 ALUMINUM ALLOY CASTINGS@ SAND 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
  • 1959 SAE AMS4217D-1959 ALUMINUM ALLOY CASTINGS@ SAND 7Si - 0.3Mg (356-T6)
  • 1959 SAE AMS4217C-1959 ALUMINUM ALLOY CASTINGS@ SAND 7Si - 0.3Mg (356-T6)
  • 1951 SAE AMS4217B-1951 ALUMINUM ALLOY CASTINGS@ SAND 7Si - 0.3Mg (356-T6) Solution and Precipitation Treated
  • 1945 SAE AMS4217A-1945 ALUMINUM ALLOY CASTINGS Sand 7 Silicon Solution and Precipitation (356-T6)
  • 1942 SAE AMS4217H-1942 Aluminum Alloy@ Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated
  • 1942 SAE AMS4217-1942 ALUMINUM ALLOY CASTINGS (Sand) 7 Silicon (356 - T6)