SAE AMS4217H-2012
Aluminum Alloy, Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated

Standard No.
SAE AMS4217H-2012
Release Date
2012
Published By
Society of Automotive Engineers (SAE)
Status
 2018-03
Replace By
SAE AMS4217J-2018
Latest
SAE AMS4217J-2018
Scope
This specification covers an aluminum alloy in the form of castings.

SAE AMS4217H-2012 history

  • 2018 SAE AMS4217J-2018 Aluminum Alloy@ Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
  • 2012 SAE AMS4217H-2012 Aluminum Alloy, Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated
  • 2007 SAE AMS4217H-2007 Aluminum Alloy, Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated UNS A03560
  • 1996 SAE AMS4217G-1996 Aluminum Alloy, Castings 7Si 0.3Mg, Solution and Precipitation Heat Treated
  • 1995 SAE AMS4217F-1995 ALUMINUM ALLOY CASTINGS, SAND 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated
  • 1986 SAE AMS4217F-1986 ALUMINUM ALLOY CASTINGS@ SAND 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
  • 1978 SAE AMS4217E-1978 ALUMINUM ALLOY CASTINGS@ SAND 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
  • 1959 SAE AMS4217D-1959 ALUMINUM ALLOY CASTINGS@ SAND 7Si - 0.3Mg (356-T6)
  • 1959 SAE AMS4217C-1959 ALUMINUM ALLOY CASTINGS@ SAND 7Si - 0.3Mg (356-T6)
  • 1951 SAE AMS4217B-1951 ALUMINUM ALLOY CASTINGS@ SAND 7Si - 0.3Mg (356-T6) Solution and Precipitation Treated
  • 1945 SAE AMS4217A-1945 ALUMINUM ALLOY CASTINGS Sand 7 Silicon Solution and Precipitation (356-T6)
  • 1942 SAE AMS4217H-1942 Aluminum Alloy@ Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated
  • 1942 SAE AMS4217-1942 ALUMINUM ALLOY CASTINGS (Sand) 7 Silicon (356 - T6)



Copyright ©2024 All Rights Reserved