SAE AMS4236A-1987
Aluminum Alloy, Castings 4.6Cu 0.35Mn 0.25Mg 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged
Home
SAE AMS4236A-1987
Standard No.
SAE AMS4236A-1987
Release Date
1987
Published By
Society of Automotive Engineers (SAE)
Status
Withdraw
Replace By
SAE AMS4236A-2000
Latest
SAE AMS4236D-2015
Scope
Primarily for components requiring high strength combined with good ductility and impact strength. Certain design and processing procedures may cause these castings to become susceptible to stress-corrosion cracking.
SAE AMS4236A-1987 history
2015
SAE AMS4236D-2015
Aluminum Alloy Castings 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged (UNS A12060)
2013
SAE AMS4236C-2013
Aluminum Alloy Castings 4.6Cu 0.35Mn 0.25Mg 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged
2007
SAE AMS4236B-2007
Aluminum Alloy Castings 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged (UNS A12060)
2000
SAE AMS4236A-2000
Aluminum Alloy Castings 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged
1987
SAE AMS4236A-1987
Aluminum Alloy, Castings 4.6Cu 0.35Mn 0.25Mg 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged
1980
SAE AMS4236-1980
ALUMINUM ALLOY CASTINGS PREMIUM GRADE 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged
Copyright ©2024 All Rights Reserved