SAE AMS4147-1968
ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.30Cr (7075-T7352) Stress Relief Compressed

Standard No.
SAE AMS4147-1968
Release Date
1968
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4147A-1978
Latest
SAE AMS4147E-2018

SAE AMS4147-1968 history

  • 2018 SAE AMS4147E-2018 Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated@ Stress Relieved by Compression@ and Overaged (UNS A97075)
  • 2012 SAE AMS4147D-2012 Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
  • 2011 SAE AMS4147B-2011 ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr(7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
  • 2007 SAE AMS4147D-2007 Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated@ Stress Relieved by Compression@ and Overaged (UNS A97075)
  • 2000 SAE AMS4147C-2000 Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr(7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
  • 1992 SAE AMS4147C-1992 Aluminum Alloy, Forgings 5.6Zn 2.5Mg 1.6Cu 0.23Cr Solution Heat Treated, Stress Relieved by Compression, and Overaged
  • 1978 SAE AMS4147A-1978 ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352)
  • 1968 SAE AMS4147-1968 ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.30Cr (7075-T7352) Stress Relief Compressed