SAE AMS4147C-2000
Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr(7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
Home
SAE AMS4147C-2000
Standard No.
SAE AMS4147C-2000
Release Date
2000
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
2012-02
Replace By
SAE AMS4147D-2007
Latest
SAE AMS4147E-2018
Scope
This specification covers an aluminum alloy in the form of die and hand forgings.
SAE AMS4147C-2000 history
2018
SAE AMS4147E-2018
Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated@ Stress Relieved by Compression@ and Overaged (UNS A97075)
2012
SAE AMS4147D-2012
Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
2011
SAE AMS4147B-2011
ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr(7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
2007
SAE AMS4147D-2007
Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated@ Stress Relieved by Compression@ and Overaged (UNS A97075)
2000
SAE AMS4147C-2000
Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr(7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged
1992
SAE AMS4147C-1992
Aluminum Alloy, Forgings 5.6Zn 2.5Mg 1.6Cu 0.23Cr Solution Heat Treated, Stress Relieved by Compression, and Overaged
1978
SAE AMS4147A-1978
ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352)
1968
SAE AMS4147-1968
ALUMINUM ALLOY FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.30Cr (7075-T7352) Stress Relief Compressed
Copyright ©2024 All Rights Reserved