ASTM B216-16
Standard Specification for Tough-Pitch Fire-Refined Copper&x2014;Refinery Shapes

Standard No.
ASTM B216-16
Release Date
2016
Published By
American Society for Testing and Materials (ASTM)
Status
Replace By
ASTM B216-22
Latest
ASTM B216-22
Scope

13.1 Calculated values shall be rounded to the nearest unit in the last right-hand significant digit used in expressing the limiting value in accordance with the rounding method in Practice E29.

1.1 This specification establishes the requirements for tough-pitch fire-refined copper wire bars, cakes, slabs, and billets for fabricating into wrought products and ingot and ingot bars for use in the manufacture of copper and copper alloy castings. This copper is not intended for electrical purposes.

1.2 Copper under this specification corresponds to the designation “FRTP” (UNS C12500) as shown in Classification B224. This copper may also be used to produce other designations of copper where the chemical composition limits are not lower then those listed for C12500 in Table 1.

1.3 Although this specification includes certain UNS designations as described in Practice E527, these designations are for cross reference only and are not specification requirements. Therefore, in case of conflict, this ASTM specification shall govern.

1.4 Units—The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.5 The following safety hazard caveat pertains only to the test method described in the annex of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and to determine the applicability of regulatory limitations prior to use.

ASTM B216-16 Referenced Document

  • ASTM B224 Standard Classification of Coppers
  • ASTM B846 Standard Terminology for Copper and Copper Alloys
  • ASTM E255 Standard Practice for Sampling Copper and Copper Alloys for the Determination of Chemical Composition
  • ASTM E29 Standard Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications
  • ASTM E50 Standard Practice for Apparatus, Reagents, and safety Precautions for Chemical Analysis of Metals
  • ASTM E527 Standard Practice for Numbering Metals and Alloys (UNS)
  • ASTM E53 Standard Test Method for Determination of Copper in Unalloyed Copper by Gravimetry

ASTM B216-16 history

  • 2022 ASTM B216-22 Standard Specification for Tough-Pitch Fire-Refined Copper—Refinery Shapes
  • 2016 ASTM B216-16 Standard Specification for Tough-Pitch Fire-Refined Copper&x2014;Refinery Shapes
  • 2010 ASTM B216-10 Standard Specification for Tough-Pitch Fire-Refined Copper&8212;Refinery Shapes
  • 1997 ASTM B216-97(2003) Standard Specification for Tough-Pitch Fire-Refined Copper8212;Refinery Shapes
  • 1997 ASTM B216-97 Standard Specification for Tough-Pitch Fire-Refined Copper Refinery Shapes