This part of EN 13674 specifies flat bottom Vignole railway rails from 27 kg/m to, but excluding 46 kg/m. Five pearlitic steel grades are specified covering a rail hardness range of 200 HBW to 390 HBW and include non-heat-treated non-alloy steels, non-heat-treated alloy steels and heat-treated non-alloy steels. There are 13 rail profiles specified in this European Standard, but these may not be available in all steel grades.
EN 13674-4:2006+A1:2009 Referenced Document
EN 10163-1:2004 Delivery requirements for surface condition of hot-rolled steel plates, wide flats and sections - Part 1: General requirements Incorporating corrigendum February 2007*, 2024-04-20 Update
EN 13674-1:2003 Railway applications - Track - Rail - Part 1: Vignole railway rails 46 kg/m and above Incorporates Amendment A1: 2007
EN ISO 6506-1:2005 Metallic Materials - Brinell Hardness Test - Part 1: Test Method ISO 6506-1:2005*, 2024-04-20 Update
EN ISO 6892-1:2009 Metallic materials - Tensile testing - Part 1: Method of test at room temperature
EN 13674-4:2006+A1:2009 history
2009EN 13674-4:2006+A1:2009 Railway applications - Track - Rail - Part 4: Vignole railway rails from 27 kg/m to, but excluding 46 kg/m
2006EN 13674-4:2006 Railway applications - Track - Rail - Part 4: Vignole railway rails from 27 kg/m to, but excluding 46 kg/m Incorporates Amendment A1: 2009