Scope
This specification covers a dilute aluminum/TiB2 metal matrix composite in the form of investment castings.

SAE AMS4471A-2014 Referenced Document

  • ASTM B557-10 Standard Test Methods for Tension Testing Wrought and Cast Aluminum- and Magnesium-Alloy Products*2024-04-20 Update
  • ASTM B557M-10 Standard Test Methods for Tension Testing Wrought and Cast Aluminum- and Magnesium-Alloy Products [Metric]*2024-04-20 Update
  • ASTM E1251-11 Standard Test Method for Analysis of Aluminum and Aluminum Alloys by Spark Atomic Emission Spectrometry*2024-04-20 Update
  • ASTM E1417-05 Standard Practice for Liquid Penetrant Testing*2024-04-20 Update
  • ASTM E155-10 Standard Reference Radiographs for Inspection of Aluminum and Magnesium Castings*2024-04-20 Update
  • ASTM E1742-08 Standard Practice for Radiographic Examination*2024-04-20 Update
  • ASTM E29-13 Standard Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications*2024-04-20 Update
  • ASTM E34-11 Standard Test Methods for Chemical Analysis of Aluminum and Aluminum-Base Alloys*2024-04-20 Update
  • ASTM E716-10 Standard Practices for Sampling and Sample Preparation of Aluminum and Aluminum Alloys for Determination of Chemical Composition by Spectrochemical Analysis*2024-04-20 Update
  • SAE AMS2175-2003 Castings, Classification and Inspection of

SAE AMS4471A-2014 history

  • 2021 SAE AMS4471B-2021 Cast Aluminum Alloy Composite 4.6Cu - 3.4Ti - 1.4B - 0.75Ag - 0.27Mg (205.0/TiB2/3p-T7P) Investment Cast, Solution and Precipitation Heat Treated
  • 2014 SAE AMS4471A-2014 Cast Aluminum Alloy Composite 4.6Cu - 3.4Ti - 1.4B - 0.75Ag - 0.27Mg (205.0/TiB2/3p-T7P) Investment Cast, Solution and Precipitation Heat Treated
  • 2012 SAE AMS4471-2012 Cast Aluminum Alloy Composite 4.6Cu 3.4Ti 1.4B 0.75Ag 0.27Mg (A205.0/TiB2/3p-T7P) Investment Cast, Solution and Precipitation Heat Treated
Cast Aluminum Alloy Composite 4.6Cu - 3.4Ti - 1.4B - 0.75Ag - 0.27Mg (205.0/TiB2/3p-T7P) Investment Cast, Solution and Precipitation Heat Treated



Copyright ©2024 All Rights Reserved