SAE AMS3209M-2014
Chloroprene (CR) Rubber, Weather Resistant, 65 - 75
Home
SAE AMS3209M-2014
Standard No.
SAE AMS3209M-2014
Release Date
2014
Published By
Society of Automotive Engineers (SAE)
Latest
SAE AMS3209M-2014
Scope
This specification covers a chloroprene (CR) rubber in the form of sheet, strip, tubing, extrusions, and molded shapes.
SAE AMS3209M-2014 Referenced Document
ASTM D2137-11
Standard Test Methods for Rubber Property
Brittleness Point of Flexible Polymers and Coated Fabrics
*
,
2024-04-20 Update
ASTM D2240-05
Standard Test Method for Rubber Property8212;Durometer Hardness
*
,
2024-04-20 Update
ASTM D395-03
Standard Test Methods for Rubber Property8212;Compression Set
*
,
2024-04-20 Update
ASTM D412-06
Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers-Tension
*
,
2024-04-20 Update
ASTM D471-12
Standard Test Method for Rubber Propertymdash;Effect of Liquids
*
,
2024-04-20 Update
ASTM D573-04
Standard Test Method for Rubber8212;Deterioration in an Air Oven
*
,
2024-04-20 Update
ASTM D624-00
Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
*
,
2024-04-20 Update
ASTM D792-13
Standard Test Methods for Density and Specific Gravity lpar;Relative Densityrpar; of Plastics by Displacement
*
,
2024-04-20 Update
ASTM D797-82
Test Method for Rubber Property-Young's Modulus at Normal and Subnormal Temperatures
SAE AMS2279
TOLERANCES Rubber Products
SAE AMS3209M-2014 history
2014
SAE AMS3209M-2014
Chloroprene (CR) Rubber, Weather Resistant, 65 - 75
2007
SAE AMS3209L-2007
Chloroprene (CR) Rubber Weather Resistant 65 - 75
1998
SAE AMS3209L-1998
Chloroprene (CR) Rubber Weather Resistant 65 - 75
1998
SAE AMS3209K-1998
Chloroprene (CR) Rubber Weather Resistant 65 - 75
1993
SAE AMS3209J-1993
Chloroprene (CR) Rubber Weather Resistant 65 - 75
1988
SAE AMS3209H-1988
Chloroprene (CR) Rubber Weather Resistant 65 - 75
1981
SAE AMS3209G-1981
CHLOROPRENE RUBBER Weather Resistant 65 - 75
1975
SAE AMS3209F-1975
CHLOROPRENE RUBBER Weather Resistant 65 - 75
1965
SAE AMS3209E-1965
SYNTHETIC RUBBER Weather Resistant, Chloroprene Type 65 - 75
1959
SAE AMS3209D-1959
SYNTHETIC RUBBER Weather Resistant, Chloroprene Type (65 - 75)
1952
SAE AMS3209C-1952
SYNTHETIC RUBBER Weather Resistant, Chloroprene Type (65-75)
1944
SAE AMS3209B-1944
SYNTHETIC RUBBER Weather Resistant-Chloroprene Type (65-75)
1943
SAE AMS3209A-1943
SYNTHETIC RUBBER Weather Resistant-Chloroprene Type (65-75)
1942
SAE AMS3209-1942
SYNTHETIC RUBBER Weather Resistant And General Purpose Application (65-75)
Copyright ©2024 All Rights Reserved