Scope
This specification covers a titanium alloy in the form of forgings and forging stock. These forgings have been used typically for parts requiring strength up to 800 °F (427 °C) and which may be welded during fabrication, but usage is not limited to such applications.

SAE AMS4966P-2013 Referenced Document

  • ASTM A255-10 Standard Test Methods for Determining Hardenability of Steel*2024-04-20 Update
  • ASTM E112-13 Standard Test Methods for Determining Average Grain Size*2024-04-20 Update
  • ASTM E1409-08 Standard Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique*2024-04-20 Update
  • ASTM E1409-13 Standard Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by Inert Gas Fusion*2024-04-20 Update
  • ASTM E1447-09 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity/Infrared Detection Method*2024-04-20 Update
  • ASTM E18-12 Standard Test Methods for Rockwell Hardness of Metallic Materials*2024-04-20 Update
  • ASTM E1941-10 Standard Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys by Combustion Analysis*2024-04-20 Update
  • ASTM E2371-04 Standard Test Method for Analysis of Titanium and Titanium Alloys by Atomic Emission Plasma Spectrometry *2024-04-20 Update
  • ASTM E2371-13 Standard Test Method for Analysis of Titanium and Titanium Alloys by Direct Current Plasma and Inductively Coupled Plasma Atomic Emission Spectrometry (Performance-Based Test Methodology)*2024-04-20 Update
  • ASTM E292-09 Standard Test Methods for Conducting Time-for-Rupture Notch Tension Tests of Materials*2024-04-20 Update
  • ASTM E350-12 Standard Test Methods for Chemical Analysis of Carbon Steel, Low-Alloy Steel, Silicon Electrical Steel, Ingot Iron, and Wrought Iron*2024-04-20 Update
  • ASTM E381-01 Standard Method of Macroetch Testing Steel Bars, Billets, Blooms, and Forgings*2024-04-20 Update
  • ASTM E384-11 Standard Test Method for Knoop and Vickers Hardness of Materials*2024-04-20 Update
  • ASTM E8-04 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-20 Update
  • ASTM E8/E8M-11 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-20 Update

SAE AMS4966P-2013 history

  • 2022 SAE AMS4966S-2022 Titanium Alloy, Forgings 5Al - 2.5Sn Annealed, 110 ksi (758 MPa) Yield Strength
  • 2017 SAE AMS4966R-2017 Titanium Alloy@ Forgings 5Al - 2.5Sn Annealed@ 110 ksi (758 MPa) Yield Strength (UNS R54520)
  • 2013 SAE AMS4966P-2013 Titanium Alloy, Forgings 5Al 2.5Sn Annealed, 110 ksi (758 MPa) Yield Strength
  • 2008 SAE AMS4966N-2008 Titanium Alloy, Forgings 5Al 2.5Sn Annealed, 110 ksi (758 MPa) Yield Strength
  • 2003 SAE AMS4966M-2003 Titanium Alloy, Forgings 5Al 2.5Sn Annealed, 110 ksi (758 MPa) Yield Strength
  • 1998 SAE AMS4966L-1998 Titanium Alloy@ Forgings 5AI - 2.5Sn Annealed@ 110 ksi (758 MPa) Yield Strength (UNS R54520)
  • 1994 SAE AMS4966K-1994 Titanium Alloy@ Forgings 5Al - 2.5Sn Annealed@ 110 ksi (758 MPa) Yield Strength (UNS R54520)
  • 1993 SAE AMS4966J-1993 TITANIUM ALLOY FORGINGS 5Al - 2.5Sn Annealed, 110,000 psi (758 MPa) Yield Strength
  • 1988 SAE AMS4966J-1988 Titanium Alloy@ Forgings 5Al - 2.5Sn Annealed@ 110@000 psi (758 MPa) Yield Strength (UNS R54520)
  • 1983 SAE AMS4966H-1983 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi (760 MPa) Yield Strength (UNS R54520)
  • 1979 SAE AMS4966G-1979 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi (758 MPa) Yield Strength (UNS R54520)
  • 1977 SAE AMS4966F-1977 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi (758 MPa) Yield Strength
  • 1972 SAE AMS4966D-1972 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi (758 MPa) Yield Strength
  • 1969 SAE AMS4966C-1969 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi Yield
  • 1966 SAE AMS4966B-1966 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi Yield
  • 1965 SAE AMS4966A-1965 Titanium Alloy Forgings 5Al - 2.5Sn Annealed@ 110@000 psi Yield
  • 1959 SAE AMS4966-1959 Titanium Alloy Forgings 5Al - 2.5Sn Annealed - 110@000 psi Yield



Copyright ©2024 All Rights Reserved