This specificaiton covers a titanium alloy in the form of forgings and forging stock. This alloy has been used typically for parts requiring strength up to 800 degree F (427 degree C), but usage is not limited to such applications.
SAE AMS4973G-2012 Referenced Document
ASTM E1409-08 Standard Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique*, 2024-04-20 Update
ASTM E1447-09 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity/Infrared Detection Method*, 2024-04-20 Update
ASTM E1941-10 Standard Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys by Combustion Analysis*, 2024-04-20 Update
ASTM E21-09 Standard Test Methods for Elevated Temperature Tension Tests of Metallic Materials*, 2024-04-20 Update
ASTM E2371-04 Standard Test Method for Analysis of Titanium and Titanium Alloys by Atomic Emission Plasma Spectrometry *, 2024-04-20 Update
ASTM E8-04 Standard Test Methods for Tension Testing of Metallic Materials*, 2024-04-20 Update
SAE AMS2249 CHEMICAL CHECK ANALYSIS LIMITS Titanium and Titanium Alloys