SAE AMS4446C-2012
Magnesium Alloy, Sand Castings 8.7Al 0.70Zn 0.26Mn Solution and Precipitation Heat Treated

Standard No.
SAE AMS4446C-2012
Release Date
2012
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4446D-2018
Latest
SAE AMS4446D-2018
Scope
This Specification covers a magnesium alloy in the form of sand castings. These castings have been used typically for parts operating up to 300 °F (149 °C), and requiring moderate strength and excellent corrosion resistance, but usage is not limited to such applications.

SAE AMS4446C-2012 Referenced Document

  • ASTM B117-11 Standard Practice for Operating Salt Spray (Fog) Apparatus*2024-04-19 Update
  • ASTM B557-10 Standard Test Methods for Tension Testing Wrought and Cast Aluminum- and Magnesium-Alloy Products*2024-04-19 Update
  • ASTM B557M-10 Standard Test Methods for Tension Testing Wrought and Cast Aluminum- and Magnesium-Alloy Products [Metric]*2024-04-19 Update
  • ASTM B660-08 Standard Practices for Packaging/Packing of Aluminum and Magnesium Products*2024-04-19 Update
  • ASTM B954-07 Standard Test Method for Analysis of Magnesium and Magnesium Alloys by Atomic Emission Spectrometry*2024-04-19 Update
  • ASTM E10-10 Standard Test Method for Brinell Hardness of Metallic Materials*2024-04-19 Update
  • ASTM E1417-05 Standard Practice for Liquid Penetrant Testing*2024-04-19 Update
  • ASTM E155-10 Standard Reference Radiographs for Inspection of Aluminum and Magnesium Castings*2024-04-19 Update
  • ASTM E1742-08 Standard Practice for Radiographic Examination*2024-04-19 Update
  • SAE AMS2175-2003 Castings, Classification and Inspection of
  • SAE AMS2360 ROOM TEMPERATURE TENSILE PROPERTIES OF CASTINGS
  • SAE AMS2475G-2009 Protective Treatments Magnesium Alloys
  • SAE AMS2694 REPAIR WELDING OF AEROSPACE CASTINGS
  • SAE AMS2768-2005 Heat Treatment of Magnesium Alloy Castings
  • SAE AMS2804 IDENTIFICATION Castings

SAE AMS4446C-2012 history

  • 1970 SAE AMS4446D-2018 Magnesium Alloy, Sand Castings 8.7Al - 0.70Zn - 0.26Mn (AZ91E-T6) Solution and Precipitation Heat Treated UNS M11919
  • 2012 SAE AMS4446C-2012 Magnesium Alloy, Sand Castings 8.7Al 0.70Zn 0.26Mn Solution and Precipitation Heat Treated
  • 2006 SAE AMS4446B-2006 Magnesium Alloy, Sand Castings 8.7Al - 0.70Zn - 0.26Mn (AZ91E-T6) Solution and Precipitation Heat Treated UNS M11919
  • 1996 SAE AMS4446A-1996 Magnesium Alloy@ Sand Castings 8.7Al - 0.70Zn - 0.26Mn (AZ91E-T6) Solution and Precipitation Heat Treated (UNS M11919)
  • 1991 SAE AMS4446-1991 MAGNESIUM ALLOY CASTINGS, SAND 8.7A1 - 0.70Zn - 0.26 Mn (AZ91E-T6) Solution and Precipitation Heat Treated
  • 1986 SAE AMS4446-1986 Magnesium Alloy Castings@ Sand 8.7Al - 0.70Zn - 0.26Mn (AZ91E-T6) Solution and Precipitation Heat Treated



Copyright ©2024 All Rights Reserved