The ring crush test correlates with edgewise compression strength of paperboard. This method is intended for paperboard between 0.28 mm (0.011 in.) and 0.61 mm (0.024 in.) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in.) and as thick as 0.76 mm (0.030 in.).