YS/T 738.1-2010
Analysis Method for aluminum hydroxide for filler- Part 1: Determination method of pH value (English Version)

Standard No.
YS/T 738.1-2010
Language
Chinese, Available in English version
Release Date
2010
Published By
Professional Standard - Non-ferrous Metal
Status
Latest
YS/T 738.1-2010
Replace By
GOST 10821-2007
Scope
This part of YS/T 738 specifies the method for determining the pH value of aluminum hydroxide for fillers. This section is applicable to the determination of pH value of aluminum hydroxide used as filler. The determination range is pH: 6.0-10.5.

YS/T 738.1-2010 history

  • 2010 YS/T 738.1-2010 Analysis Method for aluminum hydroxide for filler- Part 1: Determination method of pH value

YS/T 738.1-2010 Analysis Method for aluminum hydroxide for filler- Part 1: Determination method of pH value was changed to GOST 10821-2007 Wire made of platinum and platinum-rhodium alloys for thermoelectric temperature transducers. Specifications.

Analysis Method for aluminum hydroxide for filler- Part 1: Determination method of pH value