Scope
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of precipitation-hardening corrosion- resistant and maraging steel parts. Parts aredefined in AMS2759.1.1 ApplicationThis specification is applicable to parts made from the steels listed in Table 1.The above designations are trademark or commercial designations and are for alloy recognition only.

SAE AMS2759/3E-2008 Referenced Document

  • ASTM A380 Standard Practice for Cleaning, Descaling, and Passivation of Stainless Steel Parts, Equipment, and Systems
  • ASTM E3 Standard Practice for Preparation of Metallographic Specimens
  • ASTM E8 Standard Test Methods for Tension Testing of Metallic Materials
  • ASTM E8M Standard Test Methods for Tension Testing of Metallic Materials [Metric] *2024-04-19 Update
  • SAE AMS2759 HEAT TREATMENT OF STEEL PARTS General Requirements
  • SAE ARP1820 Chord Method of Evaluating Surface Microstructural Characteristics

SAE AMS2759/3E-2008 history

  • 2014 SAE AMS2759/3E-2014 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel parts
  • 2008 SAE AMS2759/3E-2008 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts

SAE AMS2759/3E-2008 -All Parts

SAE AMS2759-1984 HEAT TREATMENT OF STEEL PARTS General Requirements SAE AMS2759/1-1994 Heat Treatment of Carbon and Low-Alloy Steel Parts, Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/10-1999 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10A-2014 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10B-2018 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/11-2014 Stress Relief of Steel Parts SAE AMS2759/11A-2018 Stress Relief of Steel Parts SAE AMS2759/12-2007 Gaseous Nitrocarburizing@ Automatically Controlled by Potentials SAE AMS2759/12A-2007 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/12B-2018 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/13-2018 Gaseous Nitrocarburizing SAE AMS2759/1A-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1B-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1C-2000 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1D-2007 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1E-2014 Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1F-2018 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1G-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1H-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1J-2021 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/2-2011 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2A-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2B-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2C-2000 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 Ksi (1517 MPa) and Higher SAE AMS2759/2D-2007 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2E-2009 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2F-2014 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2G-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2H-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2J-2019 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2K-2021 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/3-2011 Heat Treatment, Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3A-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3B-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3C-2000 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3D-2005 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3E-2014 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel parts SAE AMS2759/3F-2015 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3G-2018 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3H-2019 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/3J-2020 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/4-2011 Heat Treatment, Austenitic Corrosion-Resistant Steel Parts SAE AMS2759/4A-1996 HEAT TREATMENT AUSTENITIC CORROSION-RESISTANT STEEL PARTS



Copyright ©2024 All Rights Reserved