ASTM D5179-98
Standard Test Method for Measuring Adhesion of Organic Coatings to Plastic Substrates by Direct Tensile Testing

Standard No.
ASTM D5179-98
Release Date
1998
Published By
American Society for Testing and Materials (ASTM)
Status
Replace By
ASTM D5179-02
Latest
ASTM D5179-16(2021)
Scope

1.1 This test method covers the laboratory determination of organic coating adhesion to plastic substrates by mounting and removing an aluminum stud from the surface of the coating and measuring the force required to break the coating/substrate bond with a tensile tester.

1.2 This test method requires that the aluminum stud be glued directly to the surface of a coated, cured panel (Fig. 1).

1.3 This test method is used to compare the adhesion of coatings to various plastic substrates, thus allowing for a quantitative comparison of various coating/substrate combinations.

ASTM D5179-98 history

  • 2021 ASTM D5179-16(2021) Standard Test Method for Measuring Adhesion of Organic Coatings in the Laboratory by Direct Tensile Method
  • 2016 ASTM D5179-16 Standard Test Method for Measuring Adhesion of Organic Coatings in the Laboratory by Direct Tensile Method
  • 2002 ASTM D5179-02(2008) Standard Test Method for Measuring Adhesion of Organic Coatings to Plastic Substrates by Direct Tensile Testing
  • 2002 ASTM D5179-02 Standard Test Method for Measuring Adhesion of Organic Coatings to Plastic Substrates by Direct Tensile Testing
  • 1998 ASTM D5179-98 Standard Test Method for Measuring Adhesion of Organic Coatings to Plastic Substrates by Direct Tensile Testing



Copyright ©2024 All Rights Reserved