ASTM D4273-05
Standard Test Methods for Polyurethane Raw Materials Determination of Primary Hydroxyl Content of Polyether Polyols

Standard No.
ASTM D4273-05
Release Date
2005
Published By
American Society for Testing and Materials (ASTM)
Status
Replace By
ASTM D4273-11
Latest
ASTM D4273-23
Scope

Measurements of primary hydroxyl content are useful for providing information regarding the relative reactivities of polyols.

1.1 Carbon-13 Nuclear Magnetic Resonance Spectroscopy(carbon-13 NMR), measures the primary hydroxyl content of ethylene oxide-propylene oxide polyethers used in preparing flexible foams. It is best suited for polyethers with primary hydroxyl contents of 10 to 90 %.

Note 18212;There is no equivalent ISO standard.

1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

ASTM D4273-05 history

  • 2023 ASTM D4273-23 Standard Test Method for Polyurethane Raw Materials: Determination of Primary Hydroxyl Content of Polyether Polyols
  • 2018 ASTM D4273-18 Standard Test Methods for Polyurethane Raw Materials Determination of Primary Hydroxyl Content of Polyether Polyols
  • 2011 ASTM D4273-11 Standard Test Method for Polyurethane Raw Materials: Determination of Primary Hydroxyl Content of Polyether Polyols
  • 2005 ASTM D4273-05 Standard Test Methods for Polyurethane Raw Materials Determination of Primary Hydroxyl Content of Polyether Polyols
  • 1999 ASTM D4273-99 Standard Test Methods for Polyurethane Raw Materials Determination of Primary Hydroxyl Content of Polyether Polyols