Scope
This specification covers the requirements for embrittlement relief (baking) of heat treated steel parts to remove hydrogen infused during plating and other chemical processing (e.g., stripping, chemical milling, pickling, and etching). This specification is applicable to parts made from carbon, low-alloy, and martensitic stainless steel heat treated to a minimum strength of 180 ksi (1241 MPa) or higher heat treated to a minimum hardness of 40 HRC or equivalent, or harder. It is also applicable to threaded fasteners made from carbon, low-alloy, or martensitic stainless steels heat treated to a minimum strength of 150 ksi (1034 MPa) or 34 HRC or equivalent, parts made from high strength precipitation hardening stainless steels other than A-286, and steel parts which have been case hardened (carburized, nitrided, nitrocarburized, or carbonitrided).

SAE AMS2759/9C-2007 history


SAE AMS2759/9C-2007 -All Parts

SAE AMS2759-1984 HEAT TREATMENT OF STEEL PARTS General Requirements SAE AMS2759/1-1994 Heat Treatment of Carbon and Low-Alloy Steel Parts, Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/10-1999 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10A-2014 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10B-2018 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/11-2014 Stress Relief of Steel Parts SAE AMS2759/11A-2018 Stress Relief of Steel Parts SAE AMS2759/12-2007 Gaseous Nitrocarburizing@ Automatically Controlled by Potentials SAE AMS2759/12A-2007 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/12B-2018 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/13-2018 Gaseous Nitrocarburizing SAE AMS2759/1A-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1B-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1C-2000 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1D-2007 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1E-2014 Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1F-2018 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1G-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1H-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1J-2021 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/2-2011 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2A-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2B-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2C-2000 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 Ksi (1517 MPa) and Higher SAE AMS2759/2D-2007 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2E-2009 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2F-2014 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2G-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2H-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2J-2019 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2K-2021 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/3-2011 Heat Treatment, Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3A-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3B-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3C-2000 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3D-2005 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3E-2014 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel parts SAE AMS2759/3F-2015 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3G-2018 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3H-2019 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/3J-2020 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/4-2011 Heat Treatment, Austenitic Corrosion-Resistant Steel Parts SAE AMS2759/4A-1996 HEAT TREATMENT AUSTENITIC CORROSION-RESISTANT STEEL PARTS



Copyright ©2024 All Rights Reserved