DIN EN 15384:2008 Packaging - Flexible aluminium tubes - Test method to determine the porosity of the internal coating; English version of DIN EN 15384:2008-01
This standard is applicable for internally coated aluminium tubes, mainly used for the packing of
pharmaceutical, cosmetic, hygiene, food or other household products.
The internal coating is used as a barrier and should avoid any contact between aluminium and the product.
This standard defines two alternative methods - copper sulphate and sodium chloride method - to detect the
electrolyte conductivity as one criterion for the quality of the internal coating.
NOTE The electrolyte conductivity of the internal coating is only one criterion for evaluation of the quality of an
internal coating. It does not give any information on the quantity or size of any pores or uncoated areas, nor any hint on
possible reactions between the aluminium tube and the product. The electrolyte conductivity should never be used as the
sole criterion for quality evaluation of the internal coating, but always with other parameters e.g. film thickness, acetone
and/or ammonia resistance and of course results of enhanced stability studies.
DIN EN 15384:2008 history
2017DIN EN 15384-1:2017 Packaging - Test method to determine the porosity of the internal coating of flexible aluminium tubes - Part 1: Sodium chloride test; German version EN 15384-1:2017
2008DIN EN 15384:2008 Packaging - Flexible aluminium tubes - Test method to determine the porosity of the internal coating; English version of DIN EN 15384:2008-01
0000 DIN EN 15384:2005
1992DIN 55436-3:1992 Packaging test; tubes made of aluminium; disposition of porosity of the inside protective lacquer; electrolytical test