SAE AMS2451/3-1998
Plating, Brush, Nickel Low Stress, Low-Hardness Deposit

Standard No.
SAE AMS2451/3-1998
Release Date
1998
Published By
Society of Automotive Engineers (SAE)
Status
 2011-04
Replace By
SAE AMS2451/3A-2006
Latest
SAE AMS2451/3D-2022
Scope
This specification covers the engineering requirements and process controls for selective plating of low-hardness, low-stress nickel by electrodeposition. It should be used, in conjunction with AMS 2451, for heat-resistant and corrosion-resistant nickel deposits. This process has been used typically to provide moderate corrosion and oxidation resistance and to repair damaged, worn, or mismachined parts requiring low residual surface stress, and service at temperatures up to 700°F (371°C) but is not limited to such applications.

SAE AMS2451/3-1998 history


SAE AMS2451/3-1998 -All Parts

SAE AMS2451-1998 Plating@ Brush General Requirements SAE AMS2451/1-1998 Plating, Brush, Nickel General Purpose SAE AMS2451/10-2002 Plating, Brush, Tin-Zinc Low Hydrogen Embrittlement SAE AMS2451/10A-2011 Plating, Brush, Tin-Zinc Low Hydrogen Embrittlement SAE AMS2451/10B-2018 Plating@ Brush@ Tin-Zinc Low Hydrogen Embrittlement SAE AMS2451/10C-2023 Plating, Brush, Tin-Zinc Low Hydrogen Embrittlement SAE AMS2451/11-2001 Plating, Brush, Cobalt SAE AMS2451/11A-2011 Plating, Brush, Cobalt SAE AMS2451/11B-2022 Plating, Brush, Cobalt SAE AMS2451/12-2011 Plating, Brush, Tin SAE AMS2451/12A-2022 Plating, Brush, Tin SAE AMS2451/13-2011 Plating, Brush, Silver SAE AMS2451/13A-2022 Plating, Brush, Silver SAE AMS2451/14-2022 Plating, Brush, Nickel-Tungsten Low Hydrogen Embrittlement SAE AMS2451/1A-2011 Plating, Brush, Nickel General Purpose SAE AMS2451/1B-2022 Plating, Brush, Nickel General Purpose SAE AMS2451/2-1998 Plating, Brush, Nickel Low Stress, Hard Deposit SAE AMS2451/2A-2011 Plating, Brush, Nickel Low Stress, Hard Deposit SAE AMS2451/2B-2022 Plating, Brush, Nickel Low Stress, Hard Deposit SAE AMS2451/3-1998 Plating, Brush, Nickel Low Stress, Low-Hardness Deposit SAE AMS2451/3A-2011 Plating, Brush, Nickel Low Stress, Low-Hardness Deposit SAE AMS2451/3B-2016 Plating@ Brush@ Nickel Low Stress@ Low-Hardness Deposit SAE AMS2451/3C-2017 Plating@ Brush@ Nickel Low Stress@ Low-Hardness Deposit SAE AMS2451/3D-2022 Plating, Brush, Nickel Low-Stress, Low-Hardness Deposit SAE AMS2451/4-1998 Plating@ Brush@ Cadmium Corrosion Protective@ Low Hydrogen Embrittlement SAE AMS2451/4A-2002 Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement SAE AMS2451/4B-2011 Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement SAE AMS2451/4C-2017 Plating@ Brush@ Cadmium Corrosion Protective@ Low Hydrogen Embrittlement SAE AMS2451/4D-2017 Plating@ Brush@ Cadmium Corrosion Protective@ Low Hydrogen Embrittlement SAE AMS2451/4E-2022 Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement SAE AMS2451/5-1998 Plating, Brush, Chromium Hard Deposit, Trivalent SAE AMS2451/5A-2011 Plating, Brush, Chromium Hard Deposit, Trivalent SAE AMS2451/5B-2017 Plating@ Brush@ Chromium Hard Deposit@ Trivalent SAE AMS2451/5C-2021 Plating, Brush, Chromium Hard Deposit, Trivalent SAE AMS2451/6-1998 Plating, Brush, Copper General Purpose SAE AMS2451/6A-2011 Plating, Brush, Copper General Purpose



Copyright ©2024 All Rights Reserved