SAE AMS4323B-2003
Aluminum Alloy, Hand Forgings 5.6Zn 2.5Mg 1.6Cu 0.23Cr (7075-T7452) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated

Standard No.
SAE AMS4323B-2003
Release Date
2003
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4323B-2008
Latest
SAE AMS4323D-2020
Scope
This specification covers an aluminum alloy in the form of hand forgings procured to inch/pound dimensions. MAM 4323 is the metric version of this AMS. These forgings have been used typically for parts requiring a high level of mechanical properties and good resistance to stress-corrosion cracking, but usage is not limited to such applications.

SAE AMS4323B-2003 Referenced Document

  • ASTM B594-02 Standard Practice for Ultrasonic Inspection of Aluminum-Alloy Wrought Products for Aerospace Applications*2024-04-18 Update
  • ASTM B660-02 Standard Practices for Packaging/Packing of Aluminum and Magnesium Products*2024-04-18 Update
  • ASTM G47-98 Standard Test Method for Determining Susceptibility to Stress-Corrosion Cracking of 2XXX and 7XXX Aluminum Alloy Products
  • SAE AMS2355G-2002 Quality Assurance, Sampling and Testing Aluminum Alloys and Magnesium Alloys Wrought Products, Except Forging Stock, and Rolled, Forged, or Flash Welded Rings
  • SAE AMS2772-1997 Heat Treatment of Aluminum Alloy Raw Materials (01 1997)
  • SAE AMS2808D-2001 Identification Forgings [Superseded: SAE AMS-STD-184A, SAE AMS-STD-184]
  • SAE AS1990-1990 Aluminum Alloy Tempers

SAE AMS4323B-2003 history

  • 2020 SAE AMS4323D-2020 Aluminum Alloy, Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7452) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 2015 SAE AMS4323C-2015 Aluminum Alloy@ Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7452) Solution Heat Treated@ Stress Relieved@ and Precipitation Heat Treated (UNS A97075)
  • 2008 SAE AMS4323B-2008 Aluminum Alloy, Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7452) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 2003 SAE AMS4323B-2003 Aluminum Alloy, Hand Forgings 5.6Zn 2.5Mg 1.6Cu 0.23Cr (7075-T7452) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 1997 SAE AMS4323A-1997 Aluminum Alloy Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075- T7452) Solution Heat Treated@ Stress Relieved@ and Precipitation Heat Treated (UNS A97075)
  • 1988 SAE AMS4323-1988 Aluminum Alloy Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075- T7452) Solution Heat Treated@ Stress Relieved@ and Precipitation Heat Treated