BS ISO 12987:2005 Carbonaceous materials for the production of aluminium - Anodes, cathodes blocks, sidewall blocks and baked ramming pastes - Determination of the thermal conductivity using a comparative method
This International Standard specifies a method for the determination of thermal conductivity of carbonaceous material in the temperature range of 20 ℃ to 60 ℃. The typical range of thermal conductivity for these materials is 2 W/(K·m) to 100 W/(K·m). This method can be used for other carbon materials, such as graphitized electrodes for other applications.