SAE AMS4090D-2000
Aluminum Alloy, Plate 5.7Zn 2.2Mg 1.6Cu 0.22Cr (7475-T651) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated

Standard No.
SAE AMS4090D-2000
Release Date
2000
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4090D-2006
Latest
SAE AMS4090G-2020
Scope
This specification covers an aluminum alloy in the form of plate. This plate has been used typically for structural applications requiring plate with high strength, moderate fatigue strength, and high fracture-toughness, but usage is not limited to such applications.

SAE AMS4090D-2000 history

  • 2020 SAE AMS4090G-2020 Aluminum Alloy, Plate 5.7Zn - 2.2Mg - 1.6Cu - 0.22Cr (7475-T651) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 2015 SAE AMS4090F-2015 Aluminum Alloy@ Plate 5.7Zn – 2.2Mg – 1.6Cu – 0.22Cr (7475-T651) Solution Heat Treated@ Stress Relieved@ and Precipitation Heat Treated (UNS A97475)
  • 2011 SAE AMS4090B-2011 ALUMINUM ALLOY PLATE 5.7Zn - 2.2Mg - 1.6Cu - 0.22Cr (7475-T651) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 2008 SAE AMS4090E-2008 Aluminum Alloy, Plate 5.7Zn 2.2Mg 1.6Cu 0.22Cr (7475-T651) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 2006 SAE AMS4090D-2006 Aluminum Alloy, Plate 5.7Zn - 2.2Mg - 1.6Cu - 0.22Cr (7475-T651) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 2000 SAE AMS4090D-2000 Aluminum Alloy, Plate 5.7Zn 2.2Mg 1.6Cu 0.22Cr (7475-T651) Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
  • 1996 SAE AMS4090C-1996 Aluminum Alloy@ Plate 5.7Zn - 2.2Mg - 1.6Cu - 0.22Cr (7475-T651) Solution Heat Treated@ Stress Relieved@ and Precipitation Heat Treated (UNS A97475)
  • 1978 SAE AMS4090A-1978 ALUMINUM ALLOY PLATE 5.7Zn - 2.2Mg - 1.6Cu - 0.22Cr (7475-T651)
  • 1976 SAE AMS4090-1976 ALUMINUM ALLOY, PLATE 5.7Zn - 2.2Mg - 1.6Cu - 0.22Cr (7475-T651)