BS 3HR 601:1989
Specification for nickel-chromium-titanium-aluminium heat-resisting alloy bar and wire for the manufacture of fasteners (maximum diameter or minor sectional dimension 30 mm) (nickel base Cr 19.5, Ti 2.2, Al 1.4)

Standard No.
BS 3HR 601:1989
Release Date
1989
Published By
British Standards Institution (BSI)
Status
 2010-11
Replace By
BS 4HR 601:2010
Latest
BS 4HR 601:2010
Scope
Bar and wire for machining, continuous cold forging or cold extrusion, or hot upset forging.

BS 3HR 601:1989 history

  • 2010 BS 4HR 601:2010 Specification for nickel-chromium-titanium-aluminium heat-resisting alloy bar and wire (maximum diameter or minor sectional dimension of 30 mm) for the manufacture of fasteners (nickel base, Cr 19.5, Ti 2.2, Al 1.4)
  • 1989 BS 3HR 601:1989 Specification for nickel-chromium-titanium-aluminium heat-resisting alloy bar and wire for the manufacture of fasteners (maximum diameter or minor sectional dimension 30 mm) (nickel base Cr 19.5, Ti 2.2, Al 1.4)
Specification for nickel-chromium-titanium-aluminium heat-resisting alloy bar and wire for the manufacture of fasteners (maximum diameter or minor sectional dimension 30 mm) (nickel base Cr 19.5, Ti 2.2, Al 1.4)