SAE AMS4285A-1978
ALUMINUM ALLOY CASTINGS@ CENTRIFUGAL 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
Home
SAE AMS4285A-1978
Standard No.
SAE AMS4285A-1978
Release Date
1978
Published By
SAE - SAE International
Status
Be replaced
1990-01
Replace By
SAE AMS4285B-1990
Latest
SAE AMS4285F-2017
Scope
Form: This specification covers an aluminium alloy in the form of centrifugal castings. Application: Primarily forintricate castings with thin walls or sections used at relatively high stresses.
SAE AMS4285A-1978 history
2017
SAE AMS4285F-2017
Aluminum Alloy Castings@ Centrifugal 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
2011
SAE AMS4285E-2011
Aluminum Alloy Castings, Centrifugal, 7.0Si 0.3Mg (356.0-T6) Solution and Precipitation Heat Treated
2008
SAE AMS4285D-2008
Aluminum Alloy Castings, Centrifugal, 7.0Si 0.3Mg (356.0-T6) Solution and Precipitation Heat Treated
2006
SAE AMS4285C-2006
Aluminum Alloy Castings, Centrifugal 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated
2001
SAE AMS4285C-2001
Aluminum Alloy Castings, Centrifugal, 7.0Si 0.3Mg (356.0-T6) Solution and Precipitation Heat Treated
1994
SAE AMS4285B-1994
ALUMINUM ALLOY CASTINGS, CENTRIFUGAL 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated
1990
SAE AMS4285B-1990
Aluminum Alloy Castings@ Centrifugal 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated
1978
SAE AMS4285A-1978
ALUMINUM ALLOY CASTINGS@ CENTRIFUGAL 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated (UNS A03560)
1954
SAE AMS4285-1954
ALUMINUM ALLOY CASTINGS@ CENTRIFUGAL 7Si - 0.3Mg (356-T6) Solution and Precipitation Treated