SAE AMS4261E-2006
Aluminum Alloy Castings, Investment 7.0Si - 0.32Mg (356.0-T51) Precipitation Heat Treated
Home
SAE AMS4261E-2006
Standard No.
SAE AMS4261E-2006
Release Date
2006
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
Replace By
SAE AMS4261F-2009
Latest
SAE AMS4261G-2017
Scope
This specification covers an aluminum alloy in the form of investment castings.
SAE AMS4261E-2006 history
2017
SAE AMS4261G-2017
Aluminum Alloy Castings@ Investment 7.0Si - 0.32Mg (356.0-T51) Precipitation Heat Treated (UNS A03560)
2009
SAE AMS4261F-2009
Aluminum Alloy, Castings, Investment 7.0Si 0.30Mg, (356.0-T51), Precipitation Heat Treated
2006
SAE AMS4261E-2006
Aluminum Alloy Castings, Investment 7.0Si - 0.32Mg (356.0-T51) Precipitation Heat Treated
1998
SAE AMS4261E-1998
Aluminum Alloy, Castings, Investment 7.0Si 0.30Mg, (356.0-T51), Precipitation Heat Treated
1991
SAE AMS4261D-1991
Aluminum Alloy Castings@ Investment 7.0Si - 0.32Mg (356.0-T51) Precipitation Heat Treated
1984
SAE AMS4261C-1984
ALUMINUM ALLOY CASTINGS@ INVESTMENT 7.0Si - 0.32Mg (356.0-T51) Precipitation Heat Treated (UNS A03560)
1978
SAE AMS4261B-1978
ALUMINUM ALLOY CASTINGS@ INVESTMENT 7.0Si - 0.30Mg (356.0-T51) Precipitation Heat Treated (UNS A03560)
1970
SAE AMS4261A-1970
ALUMINUM ALLOY CASTINGS@ INVESTMENT 7.0Si - 0.3Mg (356-T51) Precipitation Heat Treated
1964
SAE AMS4261-1964
ALUMINUM ALLOY CASTINGS@ INVESTMENT 7.0Si - 0.3Mg (356-T51) Precipitation Heat Treated
Copyright ©2024 All Rights Reserved