SAE AMS2281-1994
TRACE ELEMENT CONTROL Nickel Alloy, Cobalt Alloy, and Iron Alloy Wrought Products For High–Temperature, High–Stressed Applications

Standard No.
SAE AMS2281-1994
Release Date
1994
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS2281A-2002
Latest
SAE AMS2281B-2013
Scope
This specification establishes maximum permissible limits for elements not normally specified but which may occur in trace amounts in wrought nickel, cobalt, and iron alloy products.

SAE AMS2281-1994 history

  • 2013 SAE AMS2281B-2013 Trace Element Control Nickel Alloy, Cobalt Alloy, and Iron Alloy Wrought Products for High-Temperature, High-Stressed Applications
  • 1970 SAE AMS2281A-2007 Trace Element Control Nickel Alloy@ Cobalt Alloy@ and Iron Alloy Wrought Products for High-Temperature@ High-Stressed Applications
  • 2002 SAE AMS2281A-2002 Trace Element Control Nickel Alloy, Cobalt Alloy, and Iron Alloy Wrought Products for High-Temperature, High-Stressed Applications
  • 1994 SAE AMS2281-1994 TRACE ELEMENT CONTROL Nickel Alloy, Cobalt Alloy, and Iron Alloy Wrought Products For High–Temperature, High–Stressed Applications
  • 1989 SAE AMS2281-1989 Trace Element Control Nickel Alloy@ Cobalt Alloy@ and Iron Alloy Wrought Products for High-Temperature@ High-Stressed Applications