SAE AMS4941-1956
Titanium Tubing@ Welded Annealed -40@000 psi Yield

Standard No.
SAE AMS4941-1956
Release Date
1956
Published By
SAE - SAE International
Status
 2012-12
Replace By
SAE AMS4941A-1974
Latest
SAE AMS4941H-2023
Scope
APPLICATION: Primarily for parts requiring strength up to 400 F and oxidation resistance up to 600 F.

SAE AMS4941-1956 history

  • 1970 SAE AMS4941H-2023 Titanium Tubing, Welded 40 ksi (276 MPa) Yield Strength
  • 2017 SAE AMS4941G-2017 Titanium Tubing@ Welded 40 ksi (276 MPa) Yield Strength (UNS R50400)
  • 2012 SAE AMS4941F-2012 Titanium Tubing@ Welded 40 ksi (276 MPa) Yield Strength (UNS R50400)
  • 2008 SAE AMS4941E-2008 Titanium Tubing, Welded Annealed, 40 ksi (276 MPa) Yield Strength UNS R50400
  • 2003 SAE AMS4941D-2003 Titanium Tubing, Welded Annealed, 40 ksi (276 MPa) Yield Strength
  • 1994 SAE AMS4941C-1994 Titanium Tubing, Welded Annealed, 40,000 psi (275 MPa) Yield Strength
  • 1984 SAE AMS4941C-1984 Titanium Tubing@ Welded Annealed@ 40@000 psi (276 MPa) Yield Strength
  • 1977 SAE AMS4941B-1977 TITANIUM TUBING@ WELDED Annealed@ 40@000 psi (276 MPa) Yield Strength
  • 1974 SAE AMS4941A-1974 TITANIUM TUBING@ WELDED Annealed@ 40@000 psi (276 MPa) Yield Strength
  • 1956 SAE AMS4941-1956 Titanium Tubing@ Welded Annealed -40@000 psi Yield