SAE AMS6475B-1955
Steel@ Nitriding 1.2Cr - 3.5Ni - 0.25Mo - 1.2Al (0.21 - 0.26C)
Home
SAE AMS6475B-1955
Standard No.
SAE AMS6475B-1955
Release Date
1955
Published By
SAE - SAE International
Status
Be replaced
2012-12
Replace By
SAE AMS6475C-1968
Latest
SAE AMS6475L-2018
Scope
APPLICATION: Nitrided parts@ requiring highest surface hardness@ high core hardness@ resistance to heat@ and less distortion than parts made from steel requiring quenching to case harden.
SAE AMS6475B-1955 history
2018
SAE AMS6475L-2018
Steel@ Nitriding@ Bars@ Forgings@ and Tubing 1.1Cr - 3.5Ni - 0.25Mo - 1.2Al (0.21 - 0.26C) (UNS K52355)
2013
SAE AMS6475K-2013
Steel, Nitriding, Bars, Forgings, and Tubing 1.1Cr 3.5Ni 0.25Mo 1.2Al (0.21-0.26C)
2009
SAE AMS6475J-2009
Steel, Nitriding, Bars, Forgings, and Tubing 1.1Cr 3.5Ni 0.25Mo 1.2Al (0.21-0.26C)
2004
SAE AMS6475H-2004
Steel, Nitriding, Bars, Forgings, and Tubing 1.1Cr 3.5Ni 0.25Mo 1.25Al (0.21-0.26C)
1999
SAE AMS6475G-1999
Steel, Nitriding, Bars, Forgings, and Tubing, 1.1Cr - 3.5Ni - 0.25Mo - 1.2Al (0.21 - 0.26C) UNS K52355
1992
SAE AMS6475F-1992
Steel Bars@ Forgings@ and Tubing@ Nitriding 1.1Cr - 3.5Ni - 0.25Mo - 1.2Al (0.21 - 0.26C) (UNS K52355)
1983
SAE AMS6475E-1983
STEEL BARS@ FORGINGS@ AND TUBING@ NITRIDING 1.1Cr - 3.5Ni - 0.25Mo - 1.2Al (0.21 - 0.26C) (UNS K52355)
1975
SAE AMS6475D-1975
STEEL BARS@ FORGINGS@ AND TUBING@ NITRIDING 1.1Cr - 3.5Ni - 0.25Mo - 1.25Al (0.21 - 0.26C)
1968
SAE AMS6475C-1968
STEEL BARS@ FORGINGS@ AND TUBING@ NITRIDING 1.1Cr-3.5Ni - 0.25Mo - 1.25Al (0.21 - 0.26C)
1955
SAE AMS6475B-1955
Steel@ Nitriding 1.2Cr - 3.5Ni - 0.25Mo - 1.2Al (0.21 - 0.26C)
1951
SAE AMS6475A-1951
STEEL@ NITRIDING 3.5Ni - 1.2Cr - 0.25Mo - 1.25Al (0.21-0.26C)
1945
SAE AMS6475-1945
STEEL NITRIDING 3.5 Ni-1.2 Cr-.25 Mo-1.25 Al
Copyright ©2024 All Rights Reserved