SAE AMS4164H-2013
Aluminum Alloy, Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress-Relief Stretched, Unstraightened

Standard No.
SAE AMS4164H-2013
Release Date
2013
Published By
Society of Automotive Engineers (SAE)
Status
 2019-07
Replace By
SAE AMS4164J-2019
Latest
SAE AMS4164J-2019
Scope
This specification covers an aluminum alloy in the form of extruded bars, rods, wire, profiles, and tubing.

SAE AMS4164H-2013 history

  • 2019 SAE AMS4164J-2019 Aluminum Alloy@ Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Solution Heat Treated@ Cold Worked@ Stress-Relieved by Stretching@ Unstraightened (UNS A92024)
  • 2013 SAE AMS4164H-2013 Aluminum Alloy, Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 2003 SAE AMS4164H-2003 Aluminum Alloy, Extrusions 4.4Cu 1.5Mg 0.60Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 1998 SAE AMS4164G-1998 Aluminum Alloy@ Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress-Relief Stretched@ Unstraightened (UNS A92024)
  • 1990 SAE AMS4164F-1990 Aluminum Alloy Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress- Relief Stretched@ Unstraightened
  • 1978 SAE AMS4164E-1978 ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 1968 SAE AMS4164D-1968 ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 1964 SAE AMS4164C-1964 ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.60Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 1963 SAE AMS4164B-1963 ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.6Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 1962 SAE AMS4164A-1962 ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.6Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
  • 1960 SAE AMS4164-1960 ALUMINUM ALLOY EXTRUSIONS 4.5Cu - 1.5Mg - 0.6Mn (2O24-T3510) Stress-Relief Stretched, Unstraightened