Scope
The direct adhesion test is used to determine the adhesion strength of hot-poured asphalt crack sealant at the application temperature as specified in MP 25 and PP 85. The adhesion test is a test of fracture. The object of the test is to apply tensile forces to the interface between sealant and aluminum end pieces. Sealant is confined between two halfcylindrical aluminum end pieces. The applied force and displacement can be recorded as functions of time. Energy required to break the bond can be calculated by measuring the area under the loaddisplacement curve. This energy can be considered a measure of bonding. In addition@ the maximum force to failure can be reported as adhesion strength. This standard does not purport to address all of the safety concerns@ if any@ associated with its use. It is the responsibility of the user of this standard to establish and follow appropriate health and safety practices and determine the applicability of regulatory limitations prior to use.

T 370-2018 history

  • 2024 T/CIET 370-2024 Green and low-carbon product evaluation specification adhesive
  • 2018 T 370-2018 Standard Method of Test for Measuring Adhesion of Hot-Poured Asphalt Crack Sealant Using Direct Adhesion Tester
  • 2017 T 370-2017 Standard Method of Test for Measuring Adhesion of Hot-Poured Asphalt Crack Sealant Using Direct Adhesion Tester



Copyright ©2024 All Rights Reserved