SAE AMS3659-1966
POLYTETRAFLUOROETHYLENE EXTRUSIONS Premium Strength, Stress Relieved

Standard No.
SAE AMS3659-1966
Release Date
1966
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS3659A-1976
Latest
SAE AMS3659F-2011

SAE AMS3659-1966 history

  • 2011 SAE AMS3659F-2011 Polytetrafluoroethylene (PTFE) Extrusions, Premium Strength, Sintered and Stress-Relieved
  • 2011 SAE AMS3659B-2011 POLYTETRAFLUOROETHYLENE EXTRUSIONS Premium Strength, Stress-Relieved
  • 2010 SAE AMS3659E-2010 Polytetrafluoroethylene (PTFE) Extrusions, Premium Strength, Sintered and Stress-Relieved
  • 2008 SAE AMS3659D-2008 POLYTETRAFLUOROETHYLENE EXTRUSIONS Premium Strength, Stress-Relieved
  • 1998 SAE AMS3659C-1998 Polytetrafluoroethylene Extrusions Premium Strength, Sintered and Stress-Relieved
  • 1993 SAE AMS3659C-1993 Polytetrafluoroethylene Extrusions, Premium Strength, Sintered and Stress-Relieved
  • 1976 SAE AMS3659A-1976 POLYTETRAFLUOROETHYLENE EXTRUSIONS Premium Strength, Stress-Relieved
  • 1966 SAE AMS3659-1966 POLYTETRAFLUOROETHYLENE EXTRUSIONS Premium Strength, Stress Relieved