SAE AMS3587B-1982
PLASTIC TUBING, ELECTRICAL INSULATION Irradiated Polyolefin, Pigmented, Very Flexible, Heat-Shrinkable (Low Recovery Temperature) 2 to 1 Shrink Ratio

Standard No.
SAE AMS3587B-1982
Release Date
1982
Published By
Society of Automotive Engineers (SAE)
Status
 2013-06
Replace By
SAE AMS3587C-1989
Latest
SAE AMS3587E-2011
Scope
This specification covers an irradiated, thermally-stabilized, modified polyolefin plastic in the form of a thin-wall, heat-shrinkable tubing with a low recovery temperature.

SAE AMS3587B-1982 history

  • 2011 SAE AMS3587E-2011 Plastic Tubing, Electrical Insulation, Irradiated Polyolefin, Pigmented, Very Flexible, Heat Shrinkable Low Recovery Temperature 2 to 1 Shrink Ratio
  • 1993 SAE AMS3587D-1993 Plastic Tubing, Electrical Insulation Irradiated Polyolefin, Pigmented, Very Flexible, Heat- Shrinkable Low Recovery Temperature 2 to 1 Shrink Ratio
  • 1989 SAE AMS3587C-1989 Plastic Tubing@ Electrical Insulation Irradiated Polyolefin@ Pigmented@ Very Flexible@ Heat-Shrinkable Low Recovery Temperature 2 to 1 Shrink Ratio
  • 1982 SAE AMS3587B-1982 PLASTIC TUBING, ELECTRICAL INSULATION Irradiated Polyolefin, Pigmented, Very Flexible, Heat-Shrinkable (Low Recovery Temperature) 2 to 1 Shrink Ratio
  • 1978 SAE AMS3587A-1978 PLASTIC TUBING, ELECTRICAL INSULATION Irradiated Polyolefin, Pigmented, Very Flexible Heat Shrinkable (Low Recovery Temperature) 2 to 1 Shrink Ratio
  • 1969 SAE AMS3587-1969 PLASTIC TUBING, ELECTRICAL INSULATION Irradiated Polyolefin, Pigmented, Very Flexible, Heat Shrinkable (Low Recovery Temperature) 2 to 1 Shrink Ratio