Rotational viscosity (180℃)/Pa?s Penetration (25℃, 100g, 5s)/0.1mm Softening point (ball and ball method)/℃, ≥ Ductility (5℃, 5cm/min)/cm, ≥ Flash point /℃, ≥ Residue mass loss after TFOT or RTOFT/%, ≤; Penetration ratio (25℃)/%, ≥; Ductility (5℃)/cm, ≥
T/CACE 008-2016 history
1970T/CACE 008-2017 High content vulcanized rubber powder modified asphalt for road
2016T/CACE 008-2016 High content vulcanized crumb rubber modified asphalt for pavement