ARMY MIL-F-13088 A (1)-1968
FINISH, PROTECTIVE, TUNG (CHINA WOOD) OIL BASE (WOODEN COMPONENTS OF SMALL ARMS)

Standard No.
ARMY MIL-F-13088 A (1)-1968
Release Date
1968
Published By
U.S. Military Regulations and Norms
Status
Scope
Paragraph 4.5.ii Delete the second sentence and substitute: "At the end of the drying period, the t e s t specimens shall be placed in a well ventilated oven maintained at 405" f 5'F for 30 minutes, visually examined for evidence of smoking during the heating period and then removed from the oven."