YS/T 372.1-2006
Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide (English Version)

Standard No.
YS/T 372.1-2006
Language
Chinese, Available in English version
Release Date
2006
Published By
Professional Standard - Non-ferrous Metal
Latest
YS/T 372.1-2006
Replace
YS/T 375.5-1994 YS/T 375.4-1994 YS/T 374.2-1994 YS/T 372.14-1994 YS/T 372.13-1994 YS/T 372.2-1994
Scope
This standard specifies the determination method of silver content in gold, platinum and palladium alloys. This standard applies to the determination of silver content in AuAg, AuAgPt, AuAgCu, AuAgCuGd, AuAgCuNi, AuAgCuCuMn, AuAgCuMnGd, PtAg (AgPt), PdAgCu, PdAg, PdAgCo alloys. Measuring range: 15% ~ 90%.

YS/T 372.1-2006 history

  • 2006 YS/T 372.3-2006 Methods for elementary analysis of precious alloy. Determination of palladoum content. Complexometric titration using butanedione dioxime releasing EDTA
  • 1970 YS/T 372.1-1994 Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide

YS/T 372.1-2006 Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide has been changed from YS/T 375.5-1994 .

YS/T 372.1-2006 Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide has been changed from YS/T 375.4-1994 .

YS/T 372.1-2006 Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide has been changed from YS/T 374.2-1994 .

YS/T 372.1-2006 Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide has been changed from YS/T 372.2-1994 Methods for elementary analysis of precious alloy. Determination of platinum content. Electricity titration using potassium permanganate.

Methods for elementary analysis of precious alloy. Determination of silver content. Potentiometer titration with potassium iodide